glasswool batts  
glasswool insulation

Product Introduction

IW-GT Glass wool tube insulation is one-piece,1000mm long hinged sections of fiberglass pipe Insulation that are opened,placed over the pipe and secured in place.It is widely used to insulate iron,copper,and other pipelines with operating temperatures between -120℃ to 400℃ in commercial &institutional buildings,and industrial facilities.

Product Performance

  • Low  thermal  conductivity
  • Low temperature can be used
  • Fire   resistance,non-combustible   A1. 
  • Stable  fiber  structure
  • Sound   absorption,noise   reduction
  • Excellent  stiffness  and  recovery characteristics

Product Specification

TypeIW-GT 48,IW-GT 64,IW-GT 76,
DiaThickness (mm)
DNINCHID2530405060708090100120
151/222ooooooo   
203/427ooooooo   
25134ooooooo   
321-1/442ooooooooo 
401-1/248ooooooooo 
50260ooooooooo 
652-1/273ooooooooo 
80389ooooooooo 
903-1/2102oooooooooo
1004114 ooooooooo
1255141 ooooooooo
1506168 ooooooooo
2008219 ooooooooo
25010273  oooooooo
30012325  oooooooo
35014356   ooooooo
40016406   ooooooo
45018457   ooooooo
50020508    oooooo
55022559     ooooo
60024610     ooooo
FacingAluminum foil,PVC,black tissue,etc.or customized finish
Noteother size please contact our sales
glasswool batts  
glasswool insulation

Technical Data

ltem NameTest MethodStandard ValueTest Value
DimensionASTMC302-13(2017) pass
  Thermalconductivity W/(m ·k)24℃   ASTMC335-17 ASTMC1045-19≤0.0360.035
93℃≤0.0450.042
204℃≤0.0650.063
260℃≤0.0780.076
371℃≤0.1110.101
Service TemperatureASTMC411-19 ASTMC417-15≤400℃396℃
Slag Resistance,max thickness changeASTMC411-19≤5.0%3.67%
Non-Fibrous (Shot)contentASTMC1335-12(2017)≤25%8.7%
Linear Shrinkable at maximumuse temperature(400℃)ASTMC356-17≤2.0%1.2%
Water Vapor Sorption By WeightASTMC1104/C1104M-13a≤5.0%0.2%
Flame Spread Index ASTME84-19a≤250
Smoke-developed Index≤500
Stress Corrosion PerformanceASTMC795-08(2013)No   crack pass